{"product_id":"3dxlabs-fr-tpu-90a","title":"3DXLABS™ FR-TPU (90A)","description":"\u003cdiv class=\"pdp-description-row\"\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\n\u003ch2\u003e3DXLABS™ FR-TPU (90A)\u003c\/h2\u003e\n\u003ch5\u003e**3DXLABS R\u0026amp;D PRODUCT**\u003c\/h5\u003e\n\u003cp\u003eFR-TPU (90A) was developed for specialized applications which not only require standard elastomeric properties, but also flame resistance. This material is halogen-free and UL94 V-0 rated at 1.5 mm, ensuring effective flame resistance without compromising health or environmental safety. With a high tear strength and heat resistance of 105°C, this material is ideal for protective sheathing or flexible parts in industries such as automation and automotive, where longevity and safety are paramount.\u003c\/p\u003e\n\u003cp\u003eAs part of our 3DXLabs R\u0026amp;D program, this material is available exclusively to our experienced users who want early access to experimental formulations and the opportunity to shape future products through direct feedback.\u003c\/p\u003e\n\u003cp\u003e3DXLabs materials are experimental and offered in limited batches. If you’re a seasoned user who wants to be at the forefront of 3D printing innovation, this is your chance to try FR-TPU (90A) and help shape its development.\u003c\/p\u003e\n\u003ch5\u003eMADE IN THE USA\u003c\/h5\u003e\n\u003cp\u003eWe manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.\u003c\/p\u003e\n\u003c\/div\u003e\n\u003cdiv class=\"pdp-description-col\"\u003e\u003cimg src=\"https:\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/FRTPU-3-web.png?v=1791386474\"\u003e\u003c\/div\u003e\n\u003c\/div\u003e","brand":"3DXTECH","offers":[{"title":"White \/ 1.75mm \/ 750g","offer_id":53977095405931,"sku":"167WT00A-750G","price":99.99,"currency_code":"USD","in_stock":true}],"thumbnail_url":"\/\/cdn.shopify.com\/s\/files\/1\/0625\/4185\/6821\/files\/FRTPU-2-web.png?v=1791386474","url":"https:\/\/www.3dxtech.com\/products\/3dxlabs-fr-tpu-90a","provider":"3DXTECH","version":"1.0","type":"link"}