Description

3DXTECH produces this 3D printing filament using a specialty compound custom-formulated using ULTEM™ 9085 resin and advanced carbon nanotube additives. ULTEM™ PEI is an amorphous, high-performance polymer that combines excellent mechanical, thermal, and chemical resistance properties. Target surface resistance: 10⁴-10⁹ Ohm

Our PEI-based filaments offer the ability to create parts with excellent properties at elevated temperatures due to a very high glass transition temperature (Tg). Ideal for use in critical applications which require electrostatic discharge (ESD) protection, a high level of cleanliness, and the outstanding thermal and chemical properties you’ve come to expect with PEI based compounds.

Benefits of 3DXSTAT ESD-PEI 9085

  • High thermal properties
  • Inherently flame resistant and self-extinguishing
  • Long-term hydrolytic stability
  • Excellent dimensional stability, low heat creep sensitivity, and a very low, uniform coefficient of thermal expansion create highly reproducible part-to-part dimensions
  • Exceptional strength and modulus, even at elevated temperatures
  • Good resistance to a broad range of chemicals, include automotive fluids, fully halogenated hydrocarbons, alcohols, and aqueous solutions
Reviews

Print Recommendations

365-390°C
Extruder Temp
360-390C
140-160°C
Bed Temp
140-160C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
120C for 4 hours
Nozzle-Abrasion

Abrasive Material

This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.

Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.

Material DETAILS

Glass Fiber Reinforced Filament

Rectangle111

What Is It?

DescriptionFibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament. This, along with their physical makeup, give this material enormous strength and mechanical properties.
Rectangle222

What Does It Do?

Glass fiber reinforcement gives material a lot of desirable properties: High strength High stiffness High chemical resistance Low thermal expansion
Rectangle333

How Does It Work?

Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.
Rectangle444

What Is It Good For?

Ideal for any applications which require strength and rigidity. For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.