Triton 3D ULTEM 1010 Black 92in3 Stratasys Compatible 3D Printer Filament
Triton ULTEM 1010
Triton ULTEM 1010
Triton ULTEM 1010
Triton 3D ULTEM 1010 Black 92in3 Stratasys Compatible 3D Printer Filament
Triton ULTEM 1010
Triton ULTEM 1010
Triton ULTEM 1010
Triton 3D ULTEM 1010 Black 92in3 Stratasys Compatible 3D Printer Filament
Triton ULTEM 1010
Triton ULTEM 1010
Triton ULTEM 1010

Triton ULTEM 1010

SKU: PEI02UN200923BK01

Regular price
$525.00
Sale price
$525.00
Regular price
$0.00
Color Code: Black
Reel Size:
In Stock
Description

Triton 3D Ultem 1010 was formulated to be 100% compatible with your Stratasys® printers and come with replacement chips but at a fraction of the cost of Stratasys® brand filament. Refill your Stratasys® printer with our alternative to Ultem 1010. This grade of Ultem 1010 is 100% guaranteed by Triton 3D® to work in your Stratasys® printers.

We manufacture this ultra-performance 3D printing filament using ULTEM™ 1010 PEI (polyether imide) resin. PEI is an amorphous, high-performance polymer that combines excellent thermal properties, exceptional dimensional stability, inherent flame retardancy, and good chemical resistance. Filaments made using ULTEM™ 1010 resin offer the ability to create parts with excellent properties at elevated temperatures due to a high glass transition temperature (Tg) of 217°C. Ultem® 1010 resin is manufactured by Sabic Innovative Polymers and is one of the leading high-performance polymers in the plastics industry. We use the same ULTEM™ PEI resin that Stratasys uses – but we charge you much less.

Don’t forget to order Stratasys Compatible Ultem 1010 Break Away Support.

We provide the EEPROM chip for your printer (Classic and Plus Style Chip).  All you need to do is load your canister, install the chip, and start printing! 

Refill and save $$$ over Stratasys® Ultem 1010.

Reviews
Nozzle-Abrasion

Abrasive Material

This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.

Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.

Material DETAILS

Glass Fiber Reinforced Filament

Rectangle111

What Is It?

DescriptionFibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament. This, along with their physical makeup, give this material enormous strength and mechanical properties.
Rectangle222

What Does It Do?

Glass fiber reinforcement gives material a lot of desirable properties: High strength High stiffness High chemical resistance Low thermal expansion
Rectangle333

How Does It Work?

Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.
Rectangle444

What Is It Good For?

Ideal for any applications which require strength and rigidity. For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.