Purple Passion ABS Filament

Hover over image to zoom

  • Purple Passion ABS Filament
  • Deep Purple ABS Filament
RRP: $29.95
$19.95 (You save $10.00)

 Product Description

Purple Passion ABS 3D Printing Filament, 1kg Reel

3DXTech™ ABS is made in the USA using 100% virgin resin and colorants - precision extruded onto 1kg reels (2.2 lbs.).  The filament is then vacuum-sealed with desiccant to protect it from moisture.  

For use with desktop printers such as Makerbot, Reprap, Printrbot jr., Makerfarm Prusa i3, MendelMax, UP! 3D, Flashforge, Solidoodle,
Afinia, Lulzbot Taz3/4, Makergear, Ultimaker, or any other printer accepting 1.75mm or 3.0mm filament.  

 

Filament diameter specs:  

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

1-3d-filament-technical-data.png

Recommended Print Conditions:

  • Extruder Temp:  220-240°C, Ideal 230°C
  • Bed Temp:  100-110°C
  • Bed Prep:  3DXTech Polyimide Tape, ABS / Acetone Slurry

 Product Reviews

You Recently Viewed...

 

Quick Links

What's News

newsletter

Follow us on

Copyright 2017 3DXTech. All Rights Reserved.
 Sitemap

Click the button below to add the Purple Passion ABS Filament to your wish list.