[Sale] ECOMAX® PLA, 3D Filament, 1 kg [Discontinued Colors]

$29.95 $24.95
(You save $5.00)

ecomax_pla_filament

ECOMAX® PLA Biopolymer is made in the USA using 100% virgin Natureworks PLA biopolymer resin and premium colorants.  Our filament is precision extruded onto 1kg reels (2.2 lbs) and then vacuum-sealed with desiccant to protect it from moisture.  

This filament is ideal for use with practically all desktop printers, such as Makerbot, Reprap, Printrbot, Prusa, UP / Afinia, Flashforge, Anet, Creality, Lulzbot, Makergear, Ultimaker, or any other printer accepting 1.75mm or 3.0mm filament.
 
Filament diameter specs:
  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm

Recommended Print Conditions:

  • Extruder Temp:  190-220°C
  • Bed Temp:  23-60°C [No Heated Bed Required]
  • Bed Prep:  3DXTech Blue Painters Tape, Hairspray, Glue Stick

DISCONTINUED COLORS