ThermaX™ High-Temp Support Filament - 500g

ThermaX™ HTS High-Temp Support

$70.00

Thermax™ High-Temp Support Filament

Our high-temp break-away support filament is ideal for use in dual extruder 3D printers designed to print high-temp materials.  ThermaX™ HTS High-Temp Support can be used as a break-away support with the following materials:

Print industrial-grade parts with Gearbox™ HT2 High-Temp 3D Printer.  Check it out HERE. 

Filament Specifications:

  • Diameter:  1.75mm, 2.85mm (+/- 0.05mm)
  • Color:  Natural 

Recommended Print Conditions: (starting points)

  • Extruder Temp: 350 - 380°C (all-metal extruder)
  • Bed Temp: 120-160°C
  • Bed Prep: Ultem® Tape, Polyimide Tape, Lightly sanded FR4 or Perf board.
  • Cooling:  No cooling fan
  • Print Speed:  Print speeds of 30mm/s (starting point).  
  • Heated Enclosure:  All high-temp materials print better within a heated enclosure or in a warm build environment.  Enclosure temp should not exceed 185°C for our HTS to remain structurally sound as a support.  
  • Support Removal:  This is a break-away support and is NOT soluble.  The support is best removed while the part is warm.  If the part cools and support removal becomes difficult, then you can heat the part in a small oven (toaster oven or similar) for 30-45 minutes; then removal will be much easier.  Chamber or oven should not exceed the Tg of the model material that you are printing with.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.