Thermax™ GT High-Temp Bio-Copolyester

Thermax™ GT High-Temp PETG [Discontinued]

$29.95

Thermax™ GT High-Temp PETG Bio-Copolyester 

THERMAX™ GT High Temperature Bio-PETG (polyethylene terephthalate glycol copolymer) is a high- temperature resistant bio-copolyester that offers an exceptionally high Tg (100°C), superior chemical resistance, and improved mechanical properties. THERMAX™ GT is BPA-free, dishwasher safe, and made using 12% biomass derived monomer.  

This filament offers higher thermal properties and chemical resistance than ABS - the bio-polymer social responsibility twist of PLA - and the low-warp excellent layer bonding you expect from PETG.  The best of all worlds wrapped up into one amazing filament.  

Diameter Specifications:

  • 1.75mm +/- 0.05mm
  • 2.85mm +/- 0.05mm  

Recommended Print Conditions:

  • Extruder Temp:  245 - 270°C
  • Bed Temp: 80-100°C
  • Bed Prep:  Hairspray or Glue Stick on Clean Glass or Build Plate
  • Support:  Our Aquatek water soluble support works great to create complex parts.  This support can be found HERE.  
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.