PEEK 3D Filament

ThermaX™ PEEK [BLACK]

$295.00

ThermaX™ PEEK 3D Filament [BLACK]

ThermaX® PEEK (PolyEtherEtherKetone) is one of the highest-performance polymers in world.  PEEK has exceptional mechanical, thermal, and chemical resistance properties making it a go-to material in some of the most demanding applications.  

Print ThermaX™ PEKK parts with Gearbox™ HT2 High-Temp 3D Printer.  Check it out HERE.

Product Attributes Include:

  • Glass Transition Temp (Tg) of 143°C 
  • Melt Temp (Tm) of 343°C 
  • Inherent flame resistance (UL94 V-0)
  • Outstanding mechanical, thermal, and chemical resistance
  • Continuous Use Temperature (CUT) of 260°C, higher for short duration
  • Excellent resistance to a broad range of chemicals, such as those used in the oil/gas, automotive, aerospace, industrial, and chemical processing industries

Filament Specifications:

  • Diameter:  1.75mm (+/- 0.05mm)
  • Color:  BLACK

Recommended Print Conditions:

  • Extruder Temp:  375 - 410°C
  • Bed Temp: 130 - 145°C
  • Bed Prep: Ultem™ Tape is the ideal build surface, glue stick on clean glass is suitable
  • Enclosure temp (if your printer is equipped):  70 - 140°C [hotter is better, up to 140°C]
  • Print Speed:  10-50 mm/s for 0.2mm layer height, fast as results dictate
  • Drying Instructions:  Please see the following instructions for when you want to dry out this filament, HERE.  

Victrex PEEK, Solvay Ketaspire PEEK, Evonik Vestakeep