Benefits of 3DXMAX PC-ABS

  • High thermal properties, with a Tg of 147C
  • Amorphous structure gives it low, near isotropic shrinkage
  • Excellent ductility and impact resistance
  • Very low odor while printing
  • Wide processing range of 280-310C
Color Code: Black
Diameter:
Reel Size:
In Stock

3DXTECH PC-ABS

3DXMAX® PC-ABS (polycarbonate + acrylonitrile butadiene styrene) is a premium high-heat 3D printing filament. PC-ABS alloys the mechanical properties & high-heat resistance of PC with the printability of ABS and allows for the printing of functional prototypes and production parts with very fine detail and excellent surface quality. 3DXMAX® Low-Gloss PC-ABS is suitable for use in both consumer-grade and industrial FDM/FFF printers that have a heated print bed. Made by 3DXTECH® in the USA.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
280-310C
140-160°C
Bed Temp
110-120C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
120C for 4+ hours