Benefits of 3DXSTAT ESD-Nylon 12

  • 3DXSTAT ESD PA12 is made using a specialty Nylon 12 (PA12) and CNT matrix that we chose for it’s printability, thermal properties, and chemical resistance. ESD PA12 is widely used in a variety of industries due to its excellent chemical resistance
  • High thermal properties, with an HDT of 150C
  • Very low moisture absorption yielding improved retention of mechanical properties even when exposed to humid environments
  • Low density makes it ideal for light-weight parts
  • Superior chemical resistances, especially when compared to PA6 and PA6/66 nylons
  • Excellent dimensional stability and reproducible part-to-part measurements
Color Code: Black
Diameter:
Reel Size:
Out Of Stock

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

3DXSTAT ESD-PA12

3DXSTAT™ ESD PA12 is made using a specialty Nylon 12 (PA12) and CNT matrix that we chose for it’s printability, thermal properties, and chemical resistance. ESD PA12 is widely used in a variety of industries due to its excellent chemical resistance, low moisture absorption, and wide processing window. Our formulation ensures very low shrinkage in the printed part resulting in excellent dimensional stability, making our ESD PA12 an excellent choice for tools, fixtures, and jigs.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
275-295C
140-160°C
Bed Temp
90-110C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
90C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.