3DXSTAT ESD-PETG is an advanced ESD-Safe compound designed for use in critical applications which require electrostatic discharge (ESD) protection. Made using cutting-edge multi-wall carbon nanotube technology, state of the art compounding technology, and precision extrusion processes. Target surface resistance: 10^4 to 10^9 Ohm. An alternative to Zortrax Z-ESD.