3DXTECH ABS
3DXTECH ABS (Acrylonitrile Butadiene Styrene) is one of the most widely used 3D printer filaments on the market, and for good reason. Our ABS is a premium mix specially formulated for 3D printing. It has excellent mechanical properties and printability, giving this material’s parts durability and a less brittle quality than other similar polymers.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.


Print Recommendations

Extruder Temp
220-240C

Bed Temp
100-110C

Heated Chamber
Recommended

Nozzle Specs
No special concerns

Layer Height
No special concerns

Drying Specs
80C for 4 hours
RECOMMENDED