ABS Pellets
ABS Pellets

3DXTECH® ABS PELLETS

SKU: 029NT00P-025K

Regular price
$437.50
Sale price
$437.50
Regular price
$0.00

Benefits of 3DXTECH® ABS PELLETS

  • If you are ordering more than 100kgs, please contact us to provide a better shipping solution.
  • Pre-dry before extrusion at 80°C for 2-4 hours.
Filament Material:
Pellet Kg Amount:
Use 3DXTECH ABS Pellets to make your own high-performance ABS filament with a home-extruder or when using a pellet-fed printer.

Processing Recommendations:

Pre-dry before extrusion at 80°C for 2-4 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
Extrusion Temp:  190 – 210°C
RECOMMENDED