Black Pellets 1
Black Pellets 1

CARBONX™ NYLON 12+CF PELLETS

SKU: 103BK00P-025K

Regular price
$1,687.50
Sale price
$1,687.50
Regular price
$0.00

Benefits of CARBONX™ NYLON 12+CF PELLETS

  • If you are ordering more than 100kgs, please contact us to provide a better shipping solution.
  • Pre-dry before extrusion at 90°C for 4-6 hours. A toaster oven works fine for this.
Filament Material:
Pellet Kg Amount:

CF15 NYLON 12 PELLETS

Ideal for home extrusion enthusiasts. Make your own CF-Nylon filament with a home-extruder such as the Filabot and Filastruder or others that are set-up for high-temp extrusion.

Processing Recommendations:

  • Pre-dry before extrusion at 90°C for 4-6 hours. A toaster oven works fine for this. Do your family a favor and do not dry the resin in your kitchen oven! (Wet material will extrude with bubbles present in the filament. If this happens, dry the resin more before processing.)
  • Extrusion Temp: 220-240°C (depending upon how your heater bands, thermocouple, and PID are configured.)
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.