CF20-PEEK
CF20-PEEK

CARBONX™ PLA+CF PELLETS

SKU: 013BK00P-025K

Regular price
$875.00
Sale price
$875.00
Regular price
$0.00

Benefits of CARBONX™ PLA+CF PELLETS

  • If you are ordering more than 100kgs, please contact us to provide a better shipping solution.
  • Pre-dry before extrusion at 50C for 4-6 hours. A toaster oven works fine for this.
Filament Material:
Pellet Kg Amount:

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CF-PLA Pellets

Ideal for home extrusion enthusiasts. Make your own CF-PLA filament with a home-extruder such as the Filabot and Filastruder or others that are set-up for high-temp extrusion.

Processing Recommendations:

  • Pre-dry before extrusion at 50C for 4-6 hours. A toaster oven works fine for this. Do your family a favor and do not dry the resin in your kitchen oven! (Wet material will extrude with bubbles present in the filament. If this happens, dry the resin more before processing.)
  • Extrusion Temp: 160-190C (depending upon how your heater bands, thermocouple, and PID are configured.)

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.