Description
CF20 PEEK Pellets [Carbon Fiber PEEK 20%]
Ideal for home extrusion enthusiasts. Â Make your own CF-PEEK filament with a home-extruder such as the Filabot and Filastruder or others that are set-up for high-temp extrusion.
Please note: Additional shipping charges may apply on orders over 10kg.
Processing Recommendations:
- Pre-dry before extrusion at 150°C for 4-6 hours. A toaster oven works fine for this. Do your family a favor and do not dry the resin in your kitchen oven! (Wet material will extrude with bubbles present in the filament. If this happens, dry the resin more before processing.)
- Extrusion Temp: 360-380°C (depending upon how your heater bands, thermocouple, and PID are configured.)
Reviews
Material DETAILS
Glass Fiber Reinforced Filament

What Is It?
DescriptionFibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament.
This, along with their physical makeup, give this material enormous strength and mechanical properties.

What Does It Do?
Glass fiber reinforcement gives material a lot of desirable properties:
High strength
High stiffness
High chemical resistance
Low thermal expansion

How Does It Work?
Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.

What Is It Good For?
Ideal for any applications which require strength and rigidity.
For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.