PLA is a
biopolymer derived from plants. Our premium blend of ECOMAX® PLA is made
right here in the USA from 100% virgin PLA Natureworks biopolymer resin and
premium colorants. It’s famous for being perfectly suited to practically all
desktop 3D printers, including the Makerbot, Prusa, Ender, Flashforge, Anet,
Creality, Lulzbot, Makergear, Ultimaker, and may more printer families. PLA is most well-known for its ease of printing, stiffness, and extremely high visual print quality. It is ideal for prototypes, concept models, and end-use printed parts for hobbyists to industry engineers alike! |
Print Recommendations

Extruder Temp
190-220C

Bed Temp
23-60C

Heated Chamber
Not required

Nozzle Specs
No special concerns

Layer Height
No special concerns

Drying Specs
45C for 4 hours
RECOMMENDED