ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA
ECOMAX PLA

ECOMAX PLA

SKU: PLA06UN104000BK01

Regular price
$120.00
Sale price
$120.00
Regular price
$0.00

Benefits of ECOMAX PLA

  • Ideal for printing without a heated bed, no enclosure required
  • Low shrinkage, warping, and easy printability, PLA prints great on practically any desktop 3D printer
  • Very low odor, perfect for 3D printing in home and office environments
  • Made from plants makes PLA a renewable biopolymer
  • Gorgeous surface quality to make printed parts look beautiful
Color Code: Black
Diameter:
Reel Size:
In Stock
PLA is a biopolymer derived from plants. Our premium blend of ECOMAX® PLA is made right here in the USA from 100% virgin PLA Natureworks biopolymer resin and premium colorants. It’s famous for being perfectly suited to practically all desktop 3D printers, including the Makerbot, Prusa, Ender, Flashforge, Anet, Creality, Lulzbot, Makergear, Ultimaker, and may more printer families.

PLA is most well-known for its ease of printing, stiffness, and extremely high visual print quality. It is ideal for prototypes, concept models, and end-use printed parts for hobbyists to industry engineers alike!

Print Recommendations

365-390°C
Extruder Temp
190-220C
140-160°C
Bed Temp
23-60C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
45C for 4 hours