HYPERLITE™ PP

SKU: 105NT00A-500G

Regular price
$58.00
Sale price
$58.00
Regular price
$0.00

Benefits of HYPERLITE™ PP

  • Excellent resistance against a huge variety of chemicals
  • Very low density, only 0.9g/cc
  • High impact and elongation, retaining the flexibility of Polypropylene
  • Easier to print than most flexible 3D printing materials, suitable for use with almost any 3D printer
  • Does not absorb moisture, no drying needed!
Color Code: Natural
Diameter:
Reel Size:
Out Of Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

HYPERLITE PP

**Special One-Time Product with Limited Stock**

HyperLite™ PP is our unfilled polypropylene that we formulated specifically for 3D printing. HyperLite™ PP is a game changer for industrial 3D printing for engineering-grade applications. The reels contain 700g of filament that gives you the freedom to print parts for drones, watercraft, automotive, or any application which would benefit from a lightweight, flexible, chemically resistant material

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
210-240°C
140-160°C
Bed Temp
60-90°C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
Not needed

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.