HYPERLITE™ PP

SKU: 105NT00A-700G

Regular price
$81.00
Sale price
$81.00
Regular price
$0.00

Benefits of HYPERLITE™ PP

  • Excellent resistance against a huge variety of chemicals
  • Very low density, only 0.9g/cc
  • High impact and elongation, retaining the flexibility of Polypropylene
  • Easier to print than most flexible 3D printing materials, suitable for use with almost any 3D printer
  • Does not absorb moisture, no drying needed!
Color Code: Natural
Diameter:
Reel Size:
In Stock

HYPERLITE PP

**Special One-Time Product with Limited Stock**

HyperLite™ PP is our unfilled polypropylene that we formulated specifically for 3D printing. HyperLite™ PP is a game changer for industrial 3D printing for engineering-grade applications. The reels contain 700g of filament that gives you the freedom to print parts for drones, watercraft, automotive, or any application which would benefit from a lightweight, flexible, chemically resistant material

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
210-240°C
140-160°C
Bed Temp
60-90°C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
Not needed
RECOMMENDED