MAX-G PETG
MAX-G PETG is a durable material that has excellent strength while remaining flexible. The base resin used in our PETG filament is FDA approved and has improved chemical resistance compared to PLA or ABS. It is suitable for cleaning with isopropyl alcohol as needed.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.


Print Recommendations

Extruder Temp
230-260C

Bed Temp
60-90C

Heated Chamber
Not required

Nozzle Specs
No special concerns

Layer Height
No special concerns

Drying Specs
65C for 4 hours