Benefits of OBSIDIAN GF+PA6

  • 9 Brilliant Colors
  • More ductile (less brittle) than CF reinforced PA6
  • 30% savings vs. Markforged Onyx™
  • Excellent strength and stiffness
  • Resistant to aliphatic hydrocarbons (oil/gas/lubricants)
  • Superior dimensional stability (low warp/shrink/CTE)
  • Compatible with Markforged FX20, X7, X5, X3, Mark Two, Onyx Pro, and Onyx One printers
Color Code: Blue
Diameter:
Reel Size:
In Stock

OBSIDIAN GF+PA6

Obsidian-GF Glass Fiber Reinforced PA6 filament was formulated to offer rich colorful options in an engineering-grade material for your Markforged printer. Obsidian-GF is a lower-cost Markforged Onyx Alternative suitable for all Markforged printers. We developed this material after extensive analysis and testing on our own in-house Markforged printer and many outside beta testers. The result is a seamless printing experience that produces parts with an outstanding appearance and excellent mechanical properties. Made using premium chopped glass fiber and PA6 copolymer, Obsidian-GF is an excellent alternative to Onyx™ that allows our customers choose brilliant colors, excellent mechanical properties, and save money when using your Markforged printer.

Don’t have a Markforged printer? That’s no problem – Obsidian™-GF is also compatible with all non-Markforged printers that are suitable for printing PA6+GF. Take advantage of the excellent strength, stiffness, and appearance of this specialty material without over spending on Markforged Onyx™.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
265-285C
140-160°C
Bed Temp
90-110C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel Nozzle
0.10mm or higher
Layer Height
.10mm or higher
65°C for 4 hours
Drying Specs
90C for 4 hours
RECOMMENDED