THERMAX PEKK A
THERMAX PEKK A
THERMAX PEKK A
THERMAX PEKK A
THERMAX PEKK A
THERMAX PEKK A

THERMAX PEKK A

SKU: PKK09UN101000BK01

Regular price
$195.00
Sale price
$195.00
Regular price
$0.00

Benefits of THERMAX PEKK A

  • High thermal properties with a CUT of 260C, Tg of 162C, and a Tm of 335C
  • Substantially easier to 3D print than PEEK
  • Wide processing window from 345-375C
  • Inherently flame resistant (UL94 V-0)
  • Low smoke generation
  • Outstanding mechanical, thermal, and chemical resistances
Color Code: Black
Diameter:
Reel Size:
In Stock

THERMAX PEKK A

ThermaX PEKK (PolyEtherKetoneKetone) is made using Arkema Kepstan PEKK and is one of the highest-performance polymers in plastics business. A leading material in the PAEK family, PEKK has exceptionally good mechanical, thermal, and chemical resistance properties. It is also not only substantially easier to print than PEEK, it’s one of the easiest ultra-polymers to 3D print period. Developed in partnership with Arkema, a leading supplier of ultra-performance materials.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
345-375C
140-160°C
Bed Temp
120-140C
Recommended
Heated Chamber
Recommended 70-150C if possible
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
120C for 4 hours
RECOMMENDED