Our break away
high-temp support filament is ideal for use in dual extruder 3D printers
designed to print high-temp materials. HTS is the premium support for our high-temp products, unlike most support filaments, which are not designed to withstand the heat required to print the top-end of performance materials. |
Print Recommendations

Extruder Temp
350-380C

Bed Temp
120-160C

Heated Chamber
Recommended no higher than 185C

Nozzle Specs
No special concerns

Layer Height
No special concerns

Drying Specs
120C for 4 hours
Product Performance Comparison
Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog
Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!

RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.