ThermaX PEEK
ThermaX PEEK (PolyEtherEtherKetone) is one of the highest-performance polymers in world. In fact, it’s one of the highest-performance plastics ever invented. PEEK has exceptional mechanical, thermal, and chemical resistance properties making it a go-to material in some of the most demanding applications where failure is not an option.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.


Print Recommendations

Extruder Temp
375-410C

Bed Temp
130-145C

Heated Chamber
Recommended 70-140C if possible

Nozzle Specs
No special concerns

Layer Height
No special concerns

Drying Specs
120C for 4 hours
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.