TPU GF30 175mm Black 500g
TPU GF30 175mm Black 500g

3DXFLEX TPU+GF30

SKU: TPU03GF300500BK00

Regular price
$68.00
Sale price
$68.00
Regular price
$0.00

Benefits of 3DXFLEX TPU+GF30

  • Shore 60D semi-flex hardness
  • Ease of printing compared to similar flexible materials
  • Excellent layer bonding
  • Outstanding fatigue resistance
  • Very low odor emitted while printing
  • Low moisture absorption
  • Retains flexibility even at low temperature
  • Styrene and BPA free
Color Code: Black
Diameter:
Reel Size:
Out Of Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

FibreX TPU+GF30

FibreX TPU+GF30 elastomer is an engineering-grade material that we chose based on its balance of printability, flexibility, chemical resistance, and toughness. 3DXFLEX TPU+GF30 has a hardness of 60D, allowing you to make very tough, impact resistant, flexible prints. We recommend direct-drive extruders, but experienced users can be successful with Bowden-type drives as well.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
230-255C
140-160°C
Bed Temp
23°-50C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
65C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.