CarbonX ezPC+CF
CarbonX ezPC+CF

CarbonX ezPC+CF

SKU: PC006CF100500BK00

Regular price
$88.00
Sale price
$88.00
Regular price
$0.00

Benefits of CarbonX ezPC+CF

  • High thermal properties, especially when reinforced with carbon fiber
  • Amorphous structure gives it low, near isotropic shrinkage (very low CTE)
  • Further improved stiffness and dimensional stability with the addition of carbon fiber reinforcement
  • Very low odor emitted while printing
  • Wide processing range of 260-280°C (suitable for most desktop printers)
  • Strongly recommend this material to be printed through a hardened steel nozzle rather than a softer metal.
Color Code: Black
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CarbonX ezPC+CF

CarbonX ezPC+CF is a high-performance carbon fiber reinforced polycarbonate filament.  This all-new material material is ideal for anyone that desires a structural component with high heat, high stiffness, excellent surface quality, and dimensional stability. ezPC+CF is a clear choice for engineering-grade projects that require excellent performance and ease of printability.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
260-280C
140-160°C
Bed Temp
80-100C
Recommended
Heated Chamber
Not Required
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
80C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.