Benefits of CarbonX PLA+CF

  • Ideal for printing without a heated bed, no enclosure required
  • Bambu AMS compatible
  • Very low odor, perfect for 3D printing in home and office environments
  • Greatly increased stiffness, modulus, and dimensional stability
  • Made from plants, PLA is a renewable biopolymer
  • Gorgeous surface quality to make printed parts look beautiful
  • Bambu AMS compatible
  • Strongly recommend this material to be printed through a hardened steel nozzle rather than a softer metal.
Color Code: Black
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CarbonX PLA+CF

CarbonX PLA+CF is an amazing bio-polymer plus recycled CF reinforced 3D printing filament. Made using 100% recycled carbon fiber and mated to the industry leading PLA bio-polymer sourced from Natureworks. This filament is ideal for anyone that desires a structural component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing. Made in the USA!

PLA is well-known for its incredible ease of printing, stiffness, and extremely high visual print quality. It’s ideal for prototyping, concept models, and end-use printed parts for hobbyists and industry engineers alike!

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
190-220 C
140-160°C
Bed Temp
23-60 C
Recommended
Heated Chamber
Not Required
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
65C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.