Benefits of FibreX ABS+GF

  • Ideal for structural engineering-grade applications
  • Exceptionally stiff and strong without being brittle
  • Excellent dimensional stability
  • Very low shrinkage, warping, or lifting, something regular un-reinforced ABS is infamous for!
  • High thermal properties allowing it to stay in use up to 98°C depending on mechanical loads applied
Color Code: Black
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

FibreX ABS+GF

FibreX ABS+GF is glass fiber reinforced ABS. It is tough as nails, very stiff, and strong allowing users to create structural parts without the lifting or warping that can happen with unfilled ABS. We use premium ABS and a special glass fiber chosen to be compatible with ABS and the FDM/FFF 3D printing process.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
230-245°C
140-160°C
Bed Temp
95-110°C
Recommended
Heated Chamber
Recommended 30-80°C if possible
0.4mm diameter minimum
Nozzle Specs
0.4mm diameter minimum Hardened Steel Nozzle
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
80°C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.