MAX-G™ PCTG
MAX-G™ PCTG
MAX-G™ PCTG
MAX-G™ PCTG
MAX-G™ PCTG
MAX-G™ PCTG
MAX-G™ PCTG
MAX-G™ PCTG
MAX-G™ PCTG

MAX-G™ PCTG

SKU: PTG07UN100750BK01

Regular price
$38.00
Sale price
$38.00
Regular price
$0.00

Benefits of MAX-G™ PCTG

  • Superior chemical resistance to ABS and PETG
  • Very low odor while printing
  • Amorphous structure giving it a low, near isotropic shrinkage
  • Low moisture absorption, 3x lower than ABS
  • Wide range of processing from 250-270C
  • Superior ductility vs. PETG
Color Code: Black
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

MAX-G™ PCTG

MAX-G PCTG is an excellent alternative to the ever-popular PETG. Both PCTG and PETG are polyesters and great printing materials, but PCTG offers improved clarity, chemical resistance and impact resistance vs. PETG – making it a more durable engineering-grade option for demanding applications. This material exhibits low shrinkage and excellent dimensional stability making it a go-to for engineering applications. PCTG does not require a heated chamber and is easily printed on most open-source desktop printers.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
250-270C
140-160°C
Bed Temp
70-90C
Recommended
Heated Chamber
Not required
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
65C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.