OBSIDIAN GF+PA6

SKU: NYL10GF101000SV01

Regular price
$130.00
Sale price
$130.00
Regular price
$0.00

Benefits of OBSIDIAN GF+PA6

  • 9 Brilliant Colors
  • More ductile (less brittle) than CF reinforced PA6
  • 30% savings vs. Markforged Onyx™
  • Excellent strength and stiffness
  • Resistant to aliphatic hydrocarbons (oil/gas/lubricants)
  • Superior dimensional stability (low warp/shrink/CTE)
  • Compatible with Markforged FX20, X7, X5, X3, Mark Two, Onyx Pro, and Onyx One printers
Color Code: Metallic Silver
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

OBSIDIAN GF+PA6

Obsidian-GF Glass Fiber Reinforced PA6 filament was formulated to offer rich colorful options in an engineering-grade material for your Markforged printer. Obsidian-GF is a lower-cost drop-in Markforged Onyx Alternative suitable for all Markforged printers. We developed this material after extensive analysis and testing on our own in-house Markforged printer and many outside beta testers. The result is a seamless printing experience that produces parts with an outstanding appearance and excellent mechanical properties. Made using premium chopped glass fiber and PA6 copolymer, Obsidian-GF is an excellent alternative to Onyx™ that allows our customers choose brilliant colors, excellent mechanical properties, and save money when using your Markforged printer.

Don’t have a Markforged printer? That’s no problem – Obsidian™-GF is also compatible with all non-Markforged printers that are suitable for printing PA6+GF. Take advantage of the excellent strength, stiffness, and appearance of this specialty material without over spending on Markforged Onyx™.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
265-285C
140-160°C
Bed Temp
90-110C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel Nozzle
0.10mm or higher
Layer Height
.10mm or higher
65°C for 4 hours
Drying Specs
90C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.