Obsidian PA6+CF
Obsidian PA6+CF

Obsidian PA6+CF

SKU: NYL13CF101000BK00

Regular price
$99.00
Sale price
$99.00
Regular price
$130.00

Benefits of Obsidian PA6+CF

  • Engineered with premium high-modulus carbon fiber and a tough PA6 copolymer base
  • Exceptional strength, stiffness, and surface finish
  • Resistant to aliphatic hydrocarbons (oil/gas/lubricants)
  • Superior dimensional stability (low warp/shrink/CTE)
  • Strongly recommend this material to be printed through a hardened steel nozzle rather than a softer metal.
Color Code: Black
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

Obsidian PA6+CF

Obsidian™ PA6+CF filament is a high-performance, carbon fiber–reinforced material designed to deliver exceptional strength, stiffness, and surface finish. Developed through extensive in-house testing and feedback from a wide network of beta users, this filament ensures a seamless printing experience with outstanding mechanical properties.

Engineered with premium high-modulus carbon fiber and a tough PA6 copolymer base, Obsidian™ provides a cost-effective solution for professionals seeking high-quality composite prints without the premium price tag.

Compatible with a wide range of 3D printers that support PA6+CF materials, Obsidian™ offers broad versatility and high value for demanding applications in engineering, prototyping, and functional part production.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
265-285C
140-160°C
Bed Temp
90-110C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel Nozzle
0.10mm or higher
Layer Height
.10mm or higher
65°C for 4 hours
Drying Specs
90C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.