ThermaX PEEK
ThermaX PEEK

ThermaX PEEK

SKU: PK001UN200250NAT0

Regular price
$158.00
Sale price
$158.00
Regular price
$0.00

Benefits of ThermaX PEEK

  • Inherently flame resistant and self-extinguishing
  • Long-term hydrolytic stability even above 250C
  • Outstanding resistance to a broad range of chemicals, including automotive fluids, fully halogenated hydrocarbons, alcohols, and aqueous solutions
  • Low smoke and toxic gas emissions
  • Excellent dimensional stability with low heat creep, low and uniform coefficient of thermal expansion, giving PEEK highly reproducible part-to-part dimensions
  • High thermal properties with a Tg of 143C, CUT of 240-260C, and Tm of 343c
Color Code: Natural
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

ThermaX PEEK

ThermaX PEEK (PolyEtherEtherKetone) is one of the highest-performance polymers in world. In fact, it’s one of the highest-performance plastics ever invented. PEEK has exceptional mechanical, thermal, and chemical resistance properties making it a go-to material in some of the most demanding applications where failure is not an option.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
375-410C
140-160°C
Bed Temp
130-145C
Recommended
Heated Chamber
Recommended 70-140C if possible
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
120C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.