Benefits of THERMAX HTS2

  • Works ideal with the following ThermaX materials: PEKK, PEEK, PEI made using ULTEM, PPSU, PSU, PPS
Color Code: Natural
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide
Our break away high-temp support filament is ideal for use in dual extruder 3D printers designed to print high-temp materials.

HTS is the premium support for our high-temp products, unlike most support filaments, which are not designed to withstand the heat required to print the top-end of performance materials.

Print Recommendations

365-390°C
Extruder Temp
350-380C
140-160°C
Bed Temp
120-160C
Recommended
Heated Chamber
Recommended no higher than 185C
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
120C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.