CF15 PEKK-A Pellets

$600.00$3,500.00

CF15 PEKK-A Pellets are ideal for Filastruder, Filabot, and Noztek type home extruders

SKU: Select options above Category:

CF15 PEKK-A Pellets [Carbon Fiber PEKK-A 15%]

Ideal for home extrusion enthusiasts.  Make your own CF-PEKK-A filament with a home-extruder such as the Filabot and Filastruder or others that are set-up for high-temp extrusion.

Please note:  Additional shipping charges may apply on orders over 10kg.

Processing Recommendations:

  • Pre-dry before extrusion at 150°C for 4-6 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  340-370°C (depending upon how your heater bands, thermocouple, and PID are configured.)