PVA Pellets
Ideal for making your own filament or for use in a pellet-fed 3D printer.
Processing Recommendations:
- Pre-dry before extrusion at 50C for 4-6 hours. A toaster oven works fine for this. Do your family a favor and do not dry the resin in your kitchen oven! Wet material will extrude with bubbles present in the filament. If this happens, dry the resin more before processing.
- Extrusion Temp: 150 - 170C depending on your extruder set-up.
- Do not cool using water tanks - this is a water soluble material and will dissolve in the water.

Have a Great Profile? Share It With the Community
Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.