Use HIPS Pellets to make your own high-performance HIPS filament with a home-extruder or when using a pellet-fed printer.

Processing Recommendations:

  • Pre-dry before extrusion at 80°C for 2-4 hours.  A toaster oven works fine for this.  Do your family a favor and do not dry the resin in your kitchen oven!  (Wet material will extrude with bubbles present in the filament.  If this happens, dry the resin more before processing.)
  • Extrusion Temp:  190 – 210°C