CarbonX ABS+CF
CarbonX ABS+CF is a high-performance carbon fiber reinforced ABS filament ideal for anyone that desires a structural component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing. Made using 10% High-Modulus Carbon Fiber. Made in the USA using premium Sabic MG-94 ABS and premium high modulus carbon fiber.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations
Extruder Temp
220-240C
Bed Temp
100-110C
Heated Chamber
Recommended
Nozzle Specs
Hardened Steel with .4mm diameter minimum
Layer Height
0.25mm or higher
Drying Specs
80C for 4 hours
Product Performance Comparison
Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.
New Digital Catalog
Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.