CeramiX PEKK
Ceramic-filled PEKK and PEEK compounds have a long history in the plastics industry – especially in the semiconductor industry where these materials have been used to machine integrated circuit (IC) test sockets and fixtures. CeramiX™ PEKK contains 15% (wt %) of high purity Alumina (Al203) which creates a hard surface ideal for repeated uses in electronics assembly and fabrication facilities. Please Note: This material was NOT formulated for applications that would create printed ‘green’ parts that would later be de-bound and sintered, leaving the ceramic additive in place.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.