DiamondBack V6 Nozzle
The team at DiamondBack recently developed a proprietary Polycrystalline Diamond (PCD) nozzle to be used in 3D printing that can handle the most challenging applications! Easier to clean and reduces tip clogging, improves layer adhesion, has a solid diamond tip, any filaments, longer life, lowers operating temperature, and delivers unmatched wear resistance!
Specifications: It is recommended that DiamondBack Nozzle users follow the operating specifications provided by each 3D printer manufacturer and each filament supplier.
DiamondBack Nozzle temperatures should not exceed 300 Celsius.
Pro Tips
- Recommended torque specs: 2.5 Nm (Newton Meter)
- Recalibrate z-offset after install to protect print bed
- Run temperature tower as optimal temperatures are typically lower
- Recommended start temperatures:
- PLA: 200°C - 215°C
- PETG: 230°C - 250°C
- PETG Carbon: 245°C - 265°C
- Maximum temperature 300°C
- Support and warranty details online at championx.com

Have a Great Profile? Share It With the Community
Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.