DiamondBack V6 Nozzle
The team at DiamondBack recently developed a proprietary Polycrystalline Diamond (PCD) nozzle to be used in 3D printing that can handle the most challenging applications! Easier to clean and reduces tip clogging, improves layer adhesion, has a solid diamond tip, any filaments, longer life, lowers operating temperature, and delivers unmatched wear resistance!
Specifications: It is recommended that DiamondBack Nozzle users follow the operating specifications provided by each 3D printer manufacturer and each filament supplier.
DiamondBack Nozzle temperatures should not exceed 300 Celsius.
Pro Tips
- Recommended torque specs: 2.5 Nm (Newton Meter)
- Recalibrate z-offset after install to protect print bed
- Run temperature tower as optimal temperatures are typically lower
- Recommended start temperatures:
- PLA: 200°C - 215°C
- PETG: 230°C - 250°C
- PETG Carbon: 245°C - 265°C
- Maximum temperature 300°C
- Support and warranty details online at championx.com

Product Performance Comparison
Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.
New Digital Catalog
Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.