MAX-G PETG
MAX-G PETG is a durable material that has excellent strength while remaining flexible. The base resin used in our PETG filament is FDA approved and has improved chemical resistance compared to PLA or ABS. It is suitable for cleaning with isopropyl alcohol as needed.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations
Extruder Temp
230-260C
Bed Temp
60-90C
Heated Chamber
Not required
Nozzle Specs
No special concerns
Layer Height
No special concerns
Drying Specs
65C for 4 hours
Product Performance Comparison
Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.
New Digital Catalog
Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.