PPE-PS 1.75mm Black 750g 3D Printer Filament
PPE-PS 1.75mm Black 750g 3D Printer Filament

ThermaX PPE+PS

SKU: PPE01UN200750BK00

Regular price
$78.00
Sale price
$78.00
Regular price
$0.00

Benefits of ThermaX PPE+PS

  • High thermal properties with an HDT of 120C
  • Flame retardant rated UL94 V-0
  • UV resistance making it suitable for outdoor applications, rated F1 per UL 746C
  • Amorphous structure granting it very low, near isotropic shrinkage
  • Excellent chemical resistance to most aqueous solutions, detergents, acids, and bases
  • Excellent long-term hydrolytic stability making it very stable in boiling water
  • Stable dielectric constant and dissipation factor over a wide range of temperatures and frequencies
Color Code: Black
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

ThermaX PPE+PS

ThermaX PPE-PS is a polyphenylene ether alloy which exhibits exceptional thermal, mechanical, and chemical resistance properties. Our PPE-PS filament is made from a UL94 V0 rated flame retardant base resin. ThermaX PPE has been an ideal material for a wide array of applications in demanding markets such as aerospace, automotive, industrial, electronics, and telecommunications.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
290-320C
140-160°C
Bed Temp
90-110C
Recommended
Heated Chamber
Recommended 50-80C if possible
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
80C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.