OBSIDIAN CF v2
In side-by-side comparisons, Obsidian™ CF v2 is now a true one-to-one alternative to Markforged’s Onyx, but at a better value.


Reformulated. Retested. Remarkable.
You spoke. We listened.
When our original Obsidian™ CF didn’t meet expectations on Markforged printers, we took your feedback seriously. We went back to the lab and reengineered the formulation from the ground up: refining the material, enhancing processability, and thoroughly testing to ensure it delivers where it counts.
The result: Obsidian™ CF v2 is a dramatically improved carbon
fiber composite that not only meets expectations but exceeds them.
- Improved mechanical performance
- Enhanced reliability and consistency
- Tested across Markforged and open-source printers.
In side-by-side comparisons, Obsidian™ CF v2 is now a true one-to-one alternative to Markforged’s Onyx, but at a better value.
Customer Tested & Approved
Product Comparison Testing
Markforged X7 Results - XY
Testing Between Onyx, Obsidian v1, Obsidian v2, & Fiberon PA-12 CF on a Markforged X7 Printer.
Product Comparison Testing
Bambu Lab X1E Results - XY
Testing Between Onyx, Obsidian v1, Obsidian v2, & Fiberon PA-12 CF on a Bambu Lab X1E printer.
Product Comparison Testing
Bambu Lab H2D Results - XY
Testing Between Onyx, Obsidian v1, Obsidian v2, & Fiberon PA-12 CF on a Bambu Lab H2D printer.
Product Comparison Testing
COMPARISON CONCLUSION
Obsidian V2 has the most consistent properties across all 3 printers which seems to show that it has consistent crystallization regardless of speed and can get Onyx level strength on any printer, not just Markforged.