Obsidian™ Glass Fiber Reinforced PA6 [Markforged ONYX Alternative]
Obsidian™-GF Glass Fiber Reinforced PA6 filament was formulated to offer rich colorful options in an engineering-grade material for your Markforged printer. Obsidian™-GF is a lower-cost drop-in Markforged Onyx Alternative suitable for all Markforged printers. We developed this material after extensive analysis and testing on our own in-house Markforged printer and many outside beta testers. The result is a seamless printing experience that produces parts with an outstanding appearance and excellent mechanical properties. Made using premium chopped glass fiber and PA6 copolymer, Obsidian™-GF is an excellent alternative to Onyx™ that allows our customers choose brilliant colors, excellent mechanical properties, and save money when using your Markforged printer.
Don’t have a Markforged printer? That’s no problem – Obsidian™-GF is also compatible with all non-Markforged printers that are suitable for printing PA6+GF. Take advantage of the excellent strength, stiffness, and appearance of this specialty material without over spending on Markforged Onyx™.
Gearbox HT2™ 3D Printer: Print industrial-grade parts using our Obsidian™ and more with the new Gearbox™ HT2 High-Temp 3D Printer.
Print Recommendations

Extruder Temp
265-285°C

Bed Temp
90-110°C

Heated Chamber
Recommended

Nozzle Specs
Hardened Steel Nozzle

Bed Adhesion
Magigoo Bed Prep

Layer Height
0.10mm or higher

Drying Specs
90°C for 4 hours

Supports
Water Soluble Supports
Benefits of Obsidian™-GF PA6+GF [Markforged Onyx Alternative]:
- Drop-in for Onyx™ without any changes required to print settings
- >9 Brilliant Colors
- >9 More ductile (less brittle) than CF reinforced PA6/li>
- >30% savings vs. Markforged Onyx™
- Excellent strength and stiffness
- Resistant to aliphatic hydrocarbons (oil/gas/lubricants)
- Superior dimensional stability (low warp/shrink/CTE)
- Compatible with Markforged FX20, X7, X5, X3, Mark Two, Onyx Pro, and Onyx One printers
Filament Specifications:
Diameter: 1.75mm +/- 0.05mm
Markforged Print Recommendations:
- Obsidian™ was formulated to be a drop-in for Onyx™ without any changes to the print settings.
Recommended Print Settings for Non-Markforged Printers:
- Extruder: 265-285°C
- Bed Temp: 90-110°C
- Nozzle: We currently recommend a hardened steel nozzle
- Bed Prep: Magigoo Bed Prep and 3DXTECH Polyimide Tape gives us the best results
- Heated Chamber: Recommended
- Supports: AquaTek™ water soluble X1 USM Universal Support Material is designed to work with complex models
- Drying Instructions: 90°C for 4 hours if the filament exhibits signs of moisture
Glass Fiber Reinforced Filament

What Is It?
Fibers made of glass reinforced into the polymer during manufacturing and aligned along the axis of filament.
This, along with their physical makeup, give this material enormous strength and mechanical properties.

What Does It Do?
Glass fiber reinforcement gives material a lot of desirable properties:
- High strength
- High stiffness
- High chemical resistance
- Low thermal expansion

How Does It Work?
Reinforcing plastic with glass fibers produces a 3D printing filament which exhibits the best properties of both fiberglass and the plastic of choice.

What Is It Good For?
Ideal for any applications which require strength and rigidity.
For these reasons, glass fiber reinforced filament is very popular in automotive, mechanical, civil engineering, and research industries.
Abrasive Material
This material is particularly abrasive among 3D printing filaments. Users may find standard brass nozzles are chewed through very quickly compared to standard wear and tear. When worn through, the nozzle diameter will widen inconsistently and the printer will experience extrusion issues.
Because of this, it's strongly recommended this material be printed through a hardened steel nozzle rather than a softer metal. Hardened steel nozzles can often be inexpensive and easily installed depending on your printer manufacturer's instructions.