3DXLABS™ EMI-ABS, Black, 1.75mm, 750g

SKU: 040BK00A-750G

Regular price
$125.00
Sale price
$125.00
Regular price
$0.00
Shipping calculated at checkout.
Out Of Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials.

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

3DXLABS™ EMI-ABS

**3DXLABS R&D PRODUCT**

Be among the first to test our latest development: EMI-ABS, a cutting-edge, electrically conductive ABS blend engineered to provide EMI shielding performance in FDM 3D printing applications.

As part of our 3DXLabs R&D program, this material is available exclusively to our experienced users who want early access to experimental formulations and the opportunity to shape future products through direct feedback.

Key Features:

  • EMI Shielding Performance:

    • Near 0 dB shielding effectiveness below 500MHz

    • Begins increasing at 600MHz, with strong performance above 700MHz

    • Between 4 dB and 16 dB shielding effectiveness from 1GHz to 9GHz, depending on infill pattern and density

  • Printability:

    • Excellent layer adhesion and surface quality when printed on Bambu X1C (no heated chamber required)

    • Heated chamber recommended to maximize mechanical strength and finish

    • Minimal warping compared to standard unfilled ABS

  • Recommended Print Settings:

    • Nozzle Temp: 285°C

    • Bed Temp: 100°C

    • Min. Chamber Temp: 60°C

    • Speed: 100 mm/s

    • Nozzle Diameter: 0.40mm, Hardened Steel

    • Min. Layer Height: 0.20mm

3DXLabs materials are experimental and offered in limited batches. If you’re a seasoned user who wants to be at the forefront of 3D printing innovation, this is your chance to try EMI-ABS and help shape its development.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.