Benefits of 3DXSTAT ESD-ABS

  • Durable and sturdy parts off practically every machine on the market
  • Easier to print than most industrial-grade materials
  • Higher melting point and thermal properties than PLA or PETG
  • Ideal for prototyping or end-use parts among both industry engineers and hobbyists alike
Color Code: Black
Diameter:
Reel Size:
In Stock

Yes, you can. Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

3DXSTAT ESD-ABS

3DXSTAT ESD ABS is an advanced ESD-Safe compound designed for use in critical applications which require electrostatic discharge (ESD) protection and a high level of cleanliness. Manufactured with consistency in mind, 3DXTECH starts with premium ABS and then compounds it according to a proprietary formulation of multi-wall carbon nanotubes – giving you a filament with excellent printing characteristics and consistent ESD properties.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
220-240°C
140-160°C
Bed Temp
100-110°C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
80°C for 4 hours

Product Performance Comparison

Explore key attributes like tensile strength, flexural strength, glass transition, and fire testing performance. Whether you're prototyping, creating functional parts, or printing detailed models, these property graphs will help you find the perfect filament for your project.

New Digital Catalog

Packed with your favorite products, detailed information, and essential technical data. Whether you’re brand new to 3-D printing, or need to find a specific filament that best fits your project, our catalog has everything you need in one easy-to-navigate place!
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.