Benefits of 3DXSTAT™ ESD-PC

  • High thermal properties including a Tg of 147C
  • Amorphous structure gives low, near isotropic shrinkage
  • Excellent ductility and impact resistance
  • Very low odor emitted while printing
  • Wide processing range of 265-300C
Color Code: Black
Diameter:
Reel Size:
Out Of Stock

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

3DXSTAT ESD-PC

3DXSTAT ESD PC is an advanced ESD-Safe compound designed for use in critical applications which require electrostatic discharge (ESD) protection. Made using cutting-edge multi-wall carbon nanotube technology, state of the art compounding technology, and precision extrusion processes. Target surface resistance of 104-109 Ohm.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
260-300C
140-160°C
Bed Temp
110-120C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
No special concerns
0.10mm or higher
Layer Height
No special concerns
65°C for 4 hours
Drying Specs
120C for 4 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.