CarbonX ABS+CF is a high-performance carbon fiber reinforced ABS filament ideal for anyone that desires a structural component with high modulus, excellent surface quality, dimensional stability, light weight, and ease of printing. Made using 10% High-Modulus Carbon Fiber. Made in the USA using premium ABS and high modulus carbon fiber.
MADE IN THE USA
We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations
Extruder Temp
220-240C
Bed Temp
100-110C
Heated Chamber
Recommended
Nozzle Specs
Hardened Steel with .4mm diameter minimum
Layer Height
0.25mm or higher
Drying Specs
80C for 4 hours
Have a Great Profile? Share It With the Community
Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED
You May Also Like
Make confident choices and discover the best printing solutions.