Benefits of CARBONX™ PEEK+CF10

  • Superior mechanical properties, even at elevated temperatures
  • Excellent chemical resistance
  • Low Coefficient of Linear Thermal Expansion (CTE)
  • Near Zero moisture absorption
  • Low smoke and toxic gas emissions
  • Always ensure the nozzle is fully purged and clear of PEEK at the end of printing. Leaving PEEK in the nozzle when cooled can result in black specks in prints and severe nozzle clogs which are difficult to clear.
Color Code: Black
Diameter:
Reel Size:
In Stock

Getting the best results starts with the right print settings. Instead of relying on one-size-fits-all recommendations, we're building a growing library of tested slicer profiles on GitHub for a wide range of printers and materials.

Our collection is continuously expanding, and if you've created a profile we don't have yet, we'd love for you to share it with the community.

See Our Print Profile Library

Our 750g reels fit within the size requirements of popular automated material management systems like the Bambu AMS, Creality CFS, and Anycubic ACE Pro. That means you can run 3DXTECH’s engineering-grade filaments in your favorite system.

Learn More

3DXTECH is now ISO 9001:2015 certified. This internationally recognized standard for quality management systems reflects a rigorous, third-party validation of how our organization establishes, maintains, and continuously improves its processes to ensure consistent quality

See our ISO 9001:2015 Certification

Weights and dimensions are close estimates. However, the exact numbers may vary slightly. Multi-material management system (MMS) compatibility is based on dimensions for a variety of systems by different manufacturers.

See Our Empty Reel Guide

CarbonX PEEK+CF10

CarbonX PEEK+CF10 is one of the premier polymers in FFF/FDM 3D Printing. Made using 10% high-modulus chopped carbon fiber for exceptional stiffness, strength, and dimensional stability.

PEEK+CF10 is one of the highest performance thermoplastics ever invented. It is used in some of the most demanding applications by industries such as Auto, Aerospace, Defense, Semi-conductor, and Oil/Gas. Engineers depend on PEEK for applications where failure is not an option.

PEEK is an advanced, ultra-high-temperature polymer that demands industrial printing conditions to achieve consistent results. Plan on a 360–450°C hot end, 120–160°C bed, and a fully enclosed, actively heated chamber (70–150°C) to control warping and ensure strong layer adhesion. Best practices also include thorough filament drying, slow print speeds, and reduced or disabled part-cooling fan. Most standard desktop printers can’t reliably maintain these conditions.

For greater success, we recommend these high performance filaments:

PEKK: Delivers similar “PEAK-family” performance benefits but is often considered more forgiving to dial in than PEEK, with improved layer bonding and reduced warping sensitivity in many setups. It’s a strong step toward PEEK-level capability without as much process difficulty.

ULTEM™ (PEI): A high-performance polymer that typically prints more predictably than PEEK while still offering excellent heat resistance and strength. It’s a great choice when you want industrial-level performance with a more manageable processing window.

PPS: Known for strong chemical resistance and dimensional stability, and it can be an easier path to consistent parts compared to PEEK. It’s a smart option for environments involving fuels, solvents, or harsh chemicals where reliability matters.

MADE IN THE USA

We manufacture all of our filaments in our 68,000 ft² manufacturing facility (located in Grand Rapids, Michigan) using state-of-the-art equipment and processes. Our goal continues to be to make the most innovative filaments on the market – targeting difficult end-use applications.

Print Recommendations

365-390°C
Extruder Temp
380-410C
Recommended
Heated Chamber
Recommended
0.4mm diameter minimum
Nozzle Specs
Hardened Steel with .4mm diameter minimum
0.10mm or higher
Layer Height
0.25mm or higher
65°C for 4 hours
Drying Specs
120C for 4 hours

Have a Great Profile? Share It With the Community

Our filament catalog is big, and printer setups are even bigger. Rather than guessing at one-size-fits-all settings, we’re building a living library of slicer profiles on GitHub. With your help, we can cover more printers, refine defaults faster, and make great results easier to achieve from the first print.
RECOMMENDED

You May Also Like

Make confident choices and discover the best printing solutions.